The austenitic-ferritic material X2CrNiMoN25-7-4 is applicated in solution annealed condition in the form of colled rolled band, warm rolled band and warm rolled sheet as well as in the form of bars, wire rod and profiles. The material is resistant to intercrystalline corrosion also in sensitized condition.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

200 GPa

Show Material materials with Elastic modulus of 200 GPa

100.0 °C

194 GPa

Show Material materials with Elastic modulus of 194 GPa

200.0 °C

186 GPa

Show Material materials with Elastic modulus of 186 GPa

300.0 °C

180 GPa

Show Material materials with Elastic modulus of 180 GPa

Elongation

20.0 °C

25 %

Show Material materials with Elongation of 25 %

Elongation, transverse

20.0 °C

20 %

Show Material materials with Elongation, transverse of 20 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Duplex Stainless Steel

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Duplex Stainless Steel

Tensile strength

20.0 °C

730 - 930 MPa

Show Material materials with Tensile strength of 730 - 930 MPa

Tensile strength, transverse

20.0 °C

730 - 930 MPa

Show Material materials with Tensile strength, transverse of 730 - 930 MPa

Yield strength Rp0.2

20.0 °C

530 MPa

Show Material materials with Yield strength Rp0.2 of 530 MPa

100.0 °C

450 MPa

Show Material materials with Yield strength Rp0.2 of 450 MPa

150.0 °C

420 MPa

Show Material materials with Yield strength Rp0.2 of 420 MPa

200.0 °C

400 MPa

Show Material materials with Yield strength Rp0.2 of 400 MPa

250.0 °C

380 MPa

Show Material materials with Yield strength Rp0.2 of 380 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K

200.0 °C

1.35E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.35E-5 1/K

300.0 °C

1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K

Unlock all property charts

Max service temperature

300 °C

Show Material materials with Max service temperature of 300 °C

Typical for Duplex Stainless Steel

Melting point

1375 - 1450 °C

Show Material materials with Melting point of 1375 - 1450 °C

Typical for Duplex Stainless Steel

Specific heat capacity

20.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

20.0 °C

15 W/(m·K)

Show Material materials with Thermal conductivity of 15 W/(m·K)

Chemical properties

PropertyValue

Carbon

0.03 %

Show Material materials with Carbon of 0.03 %

Chromium

24 - 26 %

Show Material materials with Chromium of 24 - 26 %

Manganese

2 %

Show Material materials with Manganese of 2 %

Molybdenum

3 - 4.5 %

Show Material materials with Molybdenum of 3 - 4.5 %

Nickel

6 - 8 %

Show Material materials with Nickel of 6 - 8 %

Nitrogen

0.2 - 0.35 %

Show Material materials with Nitrogen of 0.2 - 0.35 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %