Description

Related Standards

Equivalent Materials

Properties

Mechanical

Charpy impact energy aK,charpy

0 - 75 J at 20 °C

Elongation A50 A50

0 - 18 % at 20 °C

Hardness, Brinell HB

0 - 255 [-] at 20 °C

Hardness, Rockwell C HRC

0 - 24 [-] at 20 °C

Reduction of area Z

0 - 55 % at 20 °C

Tensile strength Rm

0 - 795 MPa at 20 °C

Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_

0 - 520 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cr

15 - 17.5 %

Cu

3 - 5 %

Ni

3 - 5 %

C

0 - 0.07 %

Mn

0 - 1 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.