General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 11 % Show Material materials with Elongation A50 of 11 % | |
Elongation A50, transverse | 23.0 °C | 11 % Show Material materials with Elongation A50, transverse of 11 % | |
Hardness, Brinell | 23.0 °C | 380 [-] Show Material materials with Hardness, Brinell of 380 [-] | |
Hardness, Brinell, trans | 23.0 °C | 380 [-] Show Material materials with Hardness, Brinell, trans of 380 [-] | |
Hardness, Rockwell C | 23.0 °C | 41 [-] Show Material materials with Hardness, Rockwell C of 41 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 50 % Show Material materials with Reduction of area of 50 % | |
Reduction of area, transverse | 23.0 °C | 45 % Show Material materials with Reduction of area, transverse of 45 % | |
Tensile strength | 23.0 °C | 1280 MPa Show Material materials with Tensile strength of 1280 MPa | |
Tensile strength, transverse | 23.0 °C | 1280 MPa Show Material materials with Tensile strength, transverse of 1280 MPa | |
Yield strength Rp0.2 | 23.0 °C | 1210 MPa Show Material materials with Yield strength Rp0.2 of 1210 MPa | |
Yield strength Rp0.2, transverse | 23.0 °C | 1210 MPa Show Material materials with Yield strength Rp0.2, transverse of 1210 MPa |