General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 10 % Show Material materials with Elongation A50 of 10 % | |
Elongation A50, transverse | 23.0 °C | 6 % Show Material materials with Elongation A50, transverse of 6 % | |
Hardness, Brinell | 23.0 °C | 363 [-] Show Material materials with Hardness, Brinell of 363 [-] | |
Hardness, Brinell, trans | 23.0 °C | 363 [-] Show Material materials with Hardness, Brinell, trans of 363 [-] | |
Hardness, Rockwell C | 23.0 °C | 39 [-] Show Material materials with Hardness, Rockwell C of 39 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 40 % Show Material materials with Reduction of area of 40 % | |
Reduction of area, transverse | 23.0 °C | 20 % Show Material materials with Reduction of area, transverse of 20 % | |
Tensile strength | 23.0 °C | 1240 MPa Show Material materials with Tensile strength of 1240 MPa | |
Tensile strength, transverse | 23.0 °C | 1240 MPa Show Material materials with Tensile strength, transverse of 1240 MPa | |
Yield strength Rp0.2 | 23.0 °C | 1170 MPa Show Material materials with Yield strength Rp0.2 of 1170 MPa | |
Yield strength Rp0.2, transverse | 23.0 °C | 1170 MPa Show Material materials with Yield strength Rp0.2, transverse of 1170 MPa |