ASTM A693 Grade 635 Solution-Treated

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

Mechanical

Elongation A50 A50

3 - 5 % at 20 °C

Hardness, Rockwell C HRC

32 [-] at 20 °C

Tensile strength Rm

825 MPa at 20 °C

Yield strength YS

515 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cr

16 - 17.5 %

Ni

6 - 7.5 %

Mn

1 %

Si

1 %

Al

0.4 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.