ASTM A693 Grade XM-13 Solution-Treated

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

Mechanical

Hardness, Brinell HB

363 [-] at 20 °C

Hardness, Rockwell C HRC

38 [-] at 20 °C

Chemical properties

Element

Weight %

Comment

Cr

12.3 - 13.2 %

Ni

7.5 - 8.5 %

Mo

2 - 2.5 %

Al

0.9 - 1.35 %

Mn

0.2 %

More

This material data has been provided by ASTM.