ASTM A693 Grade XM-25 Solution-Treated

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

Mechanical

Elongation A50 A50

4 % at 20 °C

Hardness, Brinell HB

255 - 311 [-] at 20 °C

Hardness, Rockwell C HRC

25 - 33 [-] at 20 °C

Tensile strength Rm

895 - 1205 MPa at 20 °C

Yield strength YS

620 - 1035 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cr

14 - 16 %

Ni

5 - 7 %

Cu

1.25 - 1.75 %

Mn

1 %

Si

1 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.