ASTM A790 Grade S32304 Heat-Treated

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperatureComment

Density

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³ at 23.0 °C

23.0 °C

Typical for Duplex Stainless Steel

Mechanical

PropertyValueTemperatureComment

Elastic modulus

200 GPa

Show Material materials with Elastic modulus of 200 GPa at 23.0 °C

23.0 °C

Typical for Duplex Stainless Steel

Elongation A50

25 %

Show Material materials with Elongation A50 of 25 % at 23.0 °C

23.0 °C

Hardness, Brinell

290 [-]

Show Material materials with Hardness, Brinell of 290 [-] at 23.0 °C

23.0 °C

Hardness, Rockwell C

30 [-]

Show Material materials with Hardness, Rockwell C of 30 [-] at 23.0 °C

23.0 °C

Poisson's ratio

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-] at 23.0 °C

23.0 °C

Typical for Duplex Stainless Steel

Shear modulus

77 GPa

Show Material materials with Shear modulus of 77 GPa at 23.0 °C

23.0 °C

Typical for Duplex Stainless Steel

Tensile strength

600 MPa

Show Material materials with Tensile strength of 600 MPa at 23.0 °C

23.0 °C

Yield strength

400 MPa

Show Material materials with Yield strength of 400 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1E-5 1/K at 23.0 °C

23.0 °C

Typical for Duplex Stainless Steel

Max service temperature

300 °C

Show Material materials with Max service temperature of 300 °C

Typical for Duplex Stainless Steel

Melting point

1375 - 1450 °C

Show Material materials with Melting point of 1375 - 1450 °C

Typical for Duplex Stainless Steel

Specific heat capacity

440 - 502 J/(kg·K)

Show Material materials with Specific heat capacity of 440 - 502 J/(kg·K) at 23.0 °C

23.0 °C

Typical for Duplex Stainless Steel

Thermal conductivity

13 - 30 W/(m·K)

Show Material materials with Thermal conductivity of 13 - 30 W/(m·K) at 23.0 °C

23.0 °C

Typical for Duplex Stainless Steel

Chemical properties

Property

Carbon

0.03 %

Chromium

21.5 - 24.5 %

Copper

0.05 - 0.6 %

Manganese

2.5 %

Molybdenum

0.05 - 0.6 %

Nickel

3 - 5.5 %

Nitrogen

0.05 - 0.2 %

Phosphorus

0.04 %

Silicon

1 %

Sulfur

0.04 %