Density ρ
8.2 g/cm³ at 20 °C
Elastic modulus E
200 GPa at 20 °C
Elongation A
6 % at 20 °C
Tensile strength Rm
2420 MPa at 20 °C
Yield strength YS
2460 MPa at 20 °C
Coefficient of thermal expansion α
1.3E-5 1/K at 20 °C
Specific heat capacity cp
440 J/(kg·K) at 20 °C
Element
Weight %
Comment
61.2 - 64.6 %
18 - 19 %
11.5 - 12.5 %
4.6 - 5.2 %
1.3 - 1.6 %