AISI 316LN Annealed

.XLSX
.PDF
Save

Properties

General

Density ρ

7.9 g/cm³ at 20 °C

Mechanical

Elastic modulus E

200 GPa at 20 °C

Elongation A

35 % at 20 °C

Tensile strength Rm

590 MPa at 20 °C

Yield strength YS

240 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

1.7E-5 1/K at 20 °C

Melting point Tm

1380 °C

Specific heat capacity cp

480 J/(kg·K) at 20 °C

Thermal conductivity λ

15 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

61.2 - 71.9 %

Cr

16 - 18.5 %

Ni

10 - 14 %

Mo

2 - 3 %

Mn

2 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.