"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.7 g/cm³

Show Material materials with Density of 7.7 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

210 GPa

Show Material materials with Elastic modulus of 210 GPa

Elongation

23.0 °C

32 %

Show Material materials with Elongation of 32 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Martensitic Stainless Steel

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Martensitic Stainless Steel

Tensile strength

23.0 °C

520 MPa

Show Material materials with Tensile strength of 520 MPa

Yield strength

23.0 °C

300 MPa

Show Material materials with Yield strength of 300 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

9.9E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.9E-6 1/K

Melting point

1480 °C

Show Material materials with Melting point of 1480 °C

Specific heat capacity

23.0 °C

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

23.0 °C

30 W/(m·K)

Show Material materials with Thermal conductivity of 30 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

6E-7 Ω·m

Show Material materials with Electrical resistivity of 6E-7 Ω·m

Typical for Martensitic Stainless Steel

Chemical properties

PropertyValue

Carbon

0 - 0.15 %

Show Material materials with Carbon of 0 - 0.15 %

Chromium

12 - 14 %

Show Material materials with Chromium of 12 - 14 %

Iron

82.4 - 87.9 %

Show Material materials with Iron of 82.4 - 87.9 %

Manganese

0 - 1.5 %

Show Material materials with Manganese of 0 - 1.5 %

Molybdenum

0 - 0.6 %

Show Material materials with Molybdenum of 0 - 0.6 %

Phosphorus

0 - 0.06 %

Show Material materials with Phosphorus of 0 - 0.06 %

Silicon

0 - 1 %

Show Material materials with Silicon of 0 - 1 %

Sulfur

0.15 - 0.35 %

Show Material materials with Sulfur of 0.15 - 0.35 %

Looking for suppliers of this material? Click to see 100 supplier of AISI 416 Annealed on Matmatch