UNS S35000 Annealed

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

220 GPa

Show Material materials with Elastic modulus of 220 GPa

Elongation

23.0 °C

14 %

Show Material materials with Elongation of 14 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

23.0 °C

1590 MPa

Show Material materials with Tensile strength of 1590 MPa

Yield strength

23.0 °C

670 MPa

Show Material materials with Yield strength of 670 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K

Specific heat capacity

23.0 °C

450 J/(kg·K)

Show Material materials with Specific heat capacity of 450 J/(kg·K)

Chemical properties

PropertyValue

Carbon

0.07 - 0.11 %

Show Material materials with Carbon of 0.07 - 0.11 %

Chromium

16 - 17 %

Show Material materials with Chromium of 16 - 17 %

Iron

72.7 - 76.9 %

Show Material materials with Iron of 72.7 - 76.9 %

Manganese

0.5 - 1.3 %

Show Material materials with Manganese of 0.5 - 1.3 %

Molybdenum

2.5 - 3.2 %

Show Material materials with Molybdenum of 2.5 - 3.2 %

Nickel

4 - 5 %

Show Material materials with Nickel of 4 - 5 %

Nitrogen

0.07 - 0.13 %

Show Material materials with Nitrogen of 0.07 - 0.13 %

Phosphorus

0 - 0.04 %

Show Material materials with Phosphorus of 0 - 0.04 %

Silicon

0 - 0.5 %

Show Material materials with Silicon of 0 - 0.5 %

Sulfur

0 - 0.03 %

Show Material materials with Sulfur of 0 - 0.03 %