General

Density

ρ

7.8 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

210 GPa at 23 °C

Show Medium Carbon Steel materials with Elastic modulus of 210 GPa at 23 °C

Elongation

A

14 % at 23 °C

Show Medium Carbon Steel materials with Elongation of 14 % at 23 °C

Poisson's ratio

ν

0.29 [-] at 23 °C

Show Medium Carbon Steel materials with Poisson's ratio of 0.29 [-] at 23 °C

Typical for Medium Carbon Steel

Shear modulus

G

75 - 80 GPa at 23 °C

Show Medium Carbon Steel materials with Shear modulus of 75 - 80 GPa at 23 °C

Typical for Carbon Steel

Tensile strength

Rm

660 MPa at 23 °C

Show Medium Carbon Steel materials with Tensile strength of 660 MPa at 23 °C

Yield strength

YS

560 MPa at 23 °C

Show Medium Carbon Steel materials with Yield strength of 560 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.2E-5 1/K at 23 °C

Max service temperature

Tmax

500 °C

Typical for Carbon Steel

Melting point

Tm

1380 - 1514 °C

Typical for Medium Carbon Steel

Specific heat capacity

cp

450 J/(kg·K) at 23 °C

Thermal conductivity

λ

21 - 52 W/(m·K) at 23 °C

Typical for Medium Carbon Steel

Electrical

Electrical resistivity

ρel

1.43E-7 - 1.74E-7 Ω·m at 23 °C

Typical for Carbon Steel

Chemical properties

Element

Weight %

Comment

Fe

98.6 - 99.05 %

Mn

0.6 - 0.9 %

C

0.35 - 0.42 %

P

0 - 0.04 %

S

0 - 0.05 %

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.