General
Property | Value | Temperature |
---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 220 GPa Show Material materials with Elastic modulus of 220 GPa at 23.0 °C | 23.0 °C | |
Elongation | 2.3 % Show Material materials with Elongation of 2.3 % at 23.0 °C | 23.0 °C | |
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] at 23.0 °C | 23.0 °C | Typical for Steel |
Tensile strength | 1310 - 1470 MPa Show Material materials with Tensile strength of 1310 - 1470 MPa at 23.0 °C | 23.0 °C | |
Yield strength | 1150 - 1190 MPa Show Material materials with Yield strength of 1150 - 1190 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K at 23.0 °C | 23.0 °C |
Specific heat capacity | 450 J/(kg·K) Show Material materials with Specific heat capacity of 450 J/(kg·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Carbon | 0.07 - 0.11 % | |
Chromium | 16 - 17 % | |
Iron | 72.7 - 76.9 % | |
Manganese | 0.5 - 1.3 % | |
Molybdenum | 2.5 - 3.2 % | |
Nickel | 4 - 5 % | |
Nitrogen | 0.07 - 0.13 % | |
Phosphorus | 0 - 0.04 % | |
Silicon | 0 - 0.5 % | |
Sulfur | 0 - 0.03 % |