See where UNS S13800 Hardened falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ7.9 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.3E-5 1/K at 23 °C
Specific heat capacity
cp450 J/(kg·K) at 23 °C
Element
Weight %
Comment
73.6 - 77.3 %
12.3 - 13.2 %
7.5 - 8.5 %
2 - 3 %
0.9 - 1.4 %
This material data has been provided by MakeItFrom.com.