UNS S17400 Hardened

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where UNS S17400 Hardened falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

7.8 g/cm³ at 20 °C

Mechanical

Elastic modulus

E

200 GPa at 20 °C

Show Precipitation Hardening Stainless Steel materials with Elastic modulus of 200 GPa at 20 °C

Elongation

A

11 - 21 % at 20 °C

Show Precipitation Hardening Stainless Steel materials with Elongation of 11 - 21 % at 20 °C

Poisson's ratio

ν

0.3 [-] at 20 °C

Show Precipitation Hardening Stainless Steel materials with Poisson's ratio of 0.3 [-] at 20 °C

Typical for Steel

Tensile strength

Rm

910 - 1410 MPa at 20 °C

Show Precipitation Hardening Stainless Steel materials with Tensile strength of 910 - 1410 MPa at 20 °C

Yield strength

YS

600 - 1260 MPa at 20 °C

Show Precipitation Hardening Stainless Steel materials with Yield strength of 600 - 1260 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

1.3E-5 1/K at 20 °C

Melting point

Tm

1400 °C

Specific heat capacity

cp

500 J/(kg·K) at 20 °C

Thermal conductivity

λ

16 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

69.6 - 79 %

Cr

15 - 17 %

Cu

3 - 5 %

Ni

3 - 5 %

C

0 - 0.07 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.