The make X5CrNiCuNb16-4 is comparable to X 5 CrNiCuNb 17 4 acc. to steel-code 1995 resp. acc. to steel-iron list 1994. The precipitation hardening steel is applicated for high strength requirements and concurrent favorable corrosion resistance, e.g. for screws, spindles and rotor disks.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

200 GPa

Show Material materials with Elastic modulus of 200 GPa

100.0 °C

195 GPa

Show Material materials with Elastic modulus of 195 GPa

200.0 °C

185 GPa

Show Material materials with Elastic modulus of 185 GPa

300.0 °C

175 GPa

Show Material materials with Elastic modulus of 175 GPa

400.0 °C

170 GPa

Show Material materials with Elastic modulus of 170 GPa

Elongation

20.0 °C

8 - 15 %

Show Material materials with Elongation of 8 - 15 %

Elongation, transverse

20.0 °C

6 - 12 %

Show Material materials with Elongation, transverse of 6 - 12 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

930 - 1300 MPa

Show Material materials with Tensile strength of 930 - 1300 MPa

Tensile strength, transverse

20.0 °C

930 - 1300 MPa

Show Material materials with Tensile strength, transverse of 930 - 1300 MPa

Yield strength Rp0.2

20.0 °C

720 - 1150 MPa

Show Material materials with Yield strength Rp0.2 of 720 - 1150 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

1.09E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.09E-5 1/K

300.0 °C

1.11E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.11E-5 1/K

Unlock all property charts

Specific heat capacity

20.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

20.0 °C

16 W/(m·K)

Show Material materials with Thermal conductivity of 16 W/(m·K)

Chemical properties

PropertyValue

Carbon

0.07 %

Show Material materials with Carbon of 0.07 %

Chromium

15 - 17 %

Show Material materials with Chromium of 15 - 17 %

Copper

3 - 5 %

Show Material materials with Copper of 3 - 5 %

Manganese

1.5 %

Show Material materials with Manganese of 1.5 %

Molybdenum

0.6 %

Show Material materials with Molybdenum of 0.6 %

Nickel

3 - 5 %

Show Material materials with Nickel of 3 - 5 %

Niobium

0.45 %

Show Material materials with Niobium of 0.45 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.7 %

Show Material materials with Silicon of 0.7 %

Sulfur

0.03 %